Selection & comparison
Processes and materials, compared side by side
The engineering trade-offs sourcing and R&D teams weigh most: heat flux, pressure drop, strength, process and sealing. The tables below put verifiable typical figures side by side to help you choose a direction — exact values follow the drawing, alloy and validation records.
Compare any two side by side
Liquid cold plates: aluminum / copper / macro-channel / micro-channel
A "what do I buy" view across four cold-plate classes — material, cooling density, pressure drop and typical fit — to pick a direction first.
| Dimension | Aluminum cold plate (6061) | Copper cold plate (Cu/OFC) | Macro-channel | Micro-channel |
|---|---|---|---|---|
| Material / conductivity | 铝 ~150–170 W/(m·K) | 铜 ~380–400 W/(m·K) | Cu/Al, larger channels | Copper, fine channels |
| Weight | Light | Heavy | Medium | Medium |
| Cooling density | Medium | Medium–high | Medium | High |
| Pressure drop | Low–medium | Low–medium | Low–medium | High |
| Clogging tolerance | Good | Good | Good | Needs filtration |
| Relative cost | Lower | Higher | Medium | High |
| Typical fit | General electronics / power devices | High-conductivity needs | Laser bars / IGBT / pumps | Very high flux / dense |
See the aluminum cold plate product
Photonics packages: optical-comms / TO / infrared / ceramic-to-metal
Different package forms in one family — choose by device, sealing and integration needs.
| Dimension | Optical-comms package | TO package | Infrared detector housing | Ceramic-to-metal package |
|---|---|---|---|---|
| Typical materials | Kovar / stainless / copper alloys | Kovar / stainless / copper alloys | Kovar / stainless / aluminum | Kovar / stainless + ceramic |
| Package / sealing | Metal housing, can be hermetic | TO-style, cap sealing | Optical-window integration | Ceramic insulator + metal seal |
| Core function | Optical device enclosure & interface | Power semiconductor / opto packaging | Carries IR detector assembly | Electrical + optical + hermetic in one |
| Common finish | Cu–Ni–Au system | Ni / Au plating | Au / anodized | Selective gold |
| Typical application | Optical modules, transceivers | Laser diodes, power devices | Thermal imaging, IR sensing | High-reliability hermetic packaging |
| Related products | Optical Communication Package Housing | TO Package Housing | Infrared Detector Housing | Ceramic-to-Metal Package Housing |
See the optical-comms package product
Liquid cold plate: micro-channel vs macro-channel
Heat flux, pressure drop and clogging tolerance — the trade-offs that decide selection.
| Dimension | Micro-channel | Macro-channel |
|---|---|---|
| Channel size | ~0.1–1 mm | Larger cross-section (a few mm) |
| Heat transfer per volume | High | Medium–low |
| Pressure drop | High (steep with narrowing) | Low–medium |
| Clogging sensitivity | High — needs filtration & clean coolant | Low |
| Manufacturing difficulty | High (fine slots, thin fins, deburr, seal) | Medium |
| Typical fit | Very high-flux devices, dense power electronics | Laser diode bars, IGBT, pump modules |
Deep dive: copper microchannel manufacturing
Cold-plate material: copper vs aluminum
Conductivity, weight, cost and coolant compatibility.
| Dimension | Copper (C11000/OFC) | Aluminum (6061) |
|---|---|---|
| Thermal conductivity | ~380–400 W/(m·K) | ~150–170 W/(m·K) |
| Density | ~8.9 g/cm³ | ~2.7 g/cm³ |
| Melting point (approx.) | ~1083 °C | ~582–652 °C |
| Linear CTE (approx.) | ~16.9 ×10⁻⁶/K | ~22.2 ×10⁻⁶/K |
| Material & machining cost | Higher | Lower |
| Typical trade-off | Best cooling; heavier, costlier | Light, cheaper, easier; lower conductivity |
Deep read: aluminum vs copper cold plates
Aluminum alloy: 6061 vs 7075
The classic strength / machinability / corrosion / cost trade.
| Dimension | 6061-T6 | 7075-T6 |
|---|---|---|
| Tensile strength (approx.) | ~310 MPa | ~570 MPa |
| Hardness (approx.) | HB ~95 | HB ~150 |
| Machinability | Excellent | Good (harder) |
| Corrosion resistance | Good | Moderate (needs anodizing) |
| Weldability | Good | Poor |
| Typical use | General structural, housings, cold plates | High-strength lightweight parts (aero/robotics) |
Anodizing: Type II vs Type III
Coating thickness, hardness and wear resistance.
| Dimension | Type II | Type III (hard) |
|---|---|---|
| Typical coating thickness | ~5–25 μm | ~25–50 μm |
| Surface hardness | Lower | High, wear-resistant |
| Wear resistance | Moderate | High |
| Dimensional impact | Small (account for build-up) | Larger (thicker build-up) |
| Typical use | Cosmetic parts, general protection | Sliding/wear/military parts |
Deep read: anodizing II vs III
Process: wire EDM vs CNC milling
Precision, throughput and geometric freedom.
| Dimension | Wire EDM | CNC milling |
|---|---|---|
| Material hardness limit | None (conductive; cuts hardened steel) | Limited by tooling |
| Typical tolerance | High (±0.005 mm class, part-dependent) | High (part-dependent) |
| 3D pockets/cavities | Poor (mainly through-profiles) | Excellent |
| Throughput | Slower | High |
| Typical use | Hardened parts, narrow slots, fine profiles | General complex 3D parts |
Deep read: wire EDM vs CNC milling
Joining: vacuum brazing vs conventional welding
Sealing, dissimilar metals and heat input.
| Dimension | Vacuum brazing | Conventional welding |
|---|---|---|
| Mechanism | Filler-based (base metal not melted) | Local base-metal melting |
| Dissimilar metals | Better suited (e.g. Cu–Kovar/stainless) | Limited |
| Heat effect / distortion | Whole-part heat, controllable | Local, but concentrated stress |
| Sealing | Can be hermetic (leak test required) | Process-dependent |
| Typical use | Hermetic housings, cold plates, vacuum parts | Structural joining |
Deep read: copper-aluminum low-temperature brazing
Not sure which route fits? Send the drawing for review
JYX reviews your material, tolerances, quantities and operating conditions and returns a manufacturable process recommendation and quote — engineering replies typically within 1–2 business days.